Epoxy resin for marble slab surface
- Feature: Epoxy Resin for Gray Marble
- Applicable material: Diano Real Gray Marble
- Epoxy system code: 4099+B25Q-KG
- Epoxy system ratio by weight: 100:25
- Curing effect: Forms a liquid sealing layer
Overview
This product is a two-component adhesive. Epoxy resin is a high-performance material used in the production of marble slabs, which can improve wear resistance, stain resistance and aesthetics. It is widely used in homes, businesses and luxury hotels to maximize the use value of marble.
Product Description
This product is a two-component adhesive. Component A consists of epoxy resin, toughening agent, and filler. Component B is a modified amine curing agent, which consists of accelerators, fillers, etc.
The good adhesion and durability of epoxy resin in marble slabs have attracted more and more attention. Epoxy resin is a high-performance material that can effectively seal fine cracks and defects on the surface of marble, thereby improving the wear resistance and anti-fouling ability of marble and improving the appearance.
Epoxy resin is often used for surface coating and repair in the production of marble slabs, thereby improving the waterproof, anti-fouling and anti-ultraviolet properties of marble. In addition, the transparency of epoxy resin helps to maintain the inherent gloss of marble. It is widely used in homes, businesses, luxury hotels and other places, and has become an important decision to maximize the use value of marble.
Product Features
| Feature | Epoxy Resin for Gray Marble |
|---|---|
| Applicable material | Diano Real Gray Marble |
| Epoxy system code | 4099+B25Q-KG |
| Epoxy system ratio by weight | 100:25 |
| Curing effect | Forms a liquid sealing layer |
| Durability | High stability and long-lasting after curing, good yellowing resistance, low viscosity, strong bonding |
| Ease of Use | Easy to mix and apply, no special tools required |
Product attributes
| Product Attributes | Description |
|---|---|
| Origin | China |
| Main Raw Material | Epoxy Resin |
| Use | Construction |
| Name | Epoxy Resin for Gray Marble |
| Category | Two-component Adhesive |
| Brand | Veropoxy |
| Adhesive Type | Resin Epoxy Resin |
| Application | Diano Real Gray Marble,Venetian Brown |
Method of operation
1.Weigh glue A and glue B using the specified weight ratio; pour into the ready clean container; twist the mixture clockwise around the container wall to mix completely; let it stand for three to five minutes before use.
2. Use glue in line with the useful time and quantity to minimize waste. Please heat glue A to 30℃ when the temperature is less than 15℃ before combining with glue B; the glue must be covered after use to prevent moisture absorption and rejection. The glue will thicken at low temperatures.
3.The surface of the cured mixture will collect air moisture and develop a layer of white mist on top when the relative humidity is higher than 85%. For room temperature curing, then, the relative humidity above 85% is not appropriate. One is advised to use heated cure.
Precautions:
Use this product in a well-ventilated area.
Keep out of reach of children and pets.
Read the product manual carefully before use.
Packaging Specifications:
25 kg container
200 kg container
1000 kg container
Shelf Life:
12 months when unopened.
Storage Conditions:
Store in a cool, dry, and well-ventilated area, away from fire and high temperatures.