Marble slab hot sale super strong adhesive epoxy resin suitable for home design

  • Feature: Epoxy Resin for Gray Marble
  • Applicable material: Diano Real Gray Marble,Venetian Brown
  • Epoxy system code: 4099+B25Q-KG
  • Epoxy system ratio by weight: 100:25
  • Curing effect: Forms a liquid sealing layer
INQUIRY

Overview

Epoxy resin is a premium two-component adhesive designed to protect and enhance marble slabs. It provides a firm protective layer, improving abrasion and chemical resistance, and highlighting the original texture and color. It is easy to apply and fixes on a smooth surface, enhancing marble’s durability and enhancing its appeal in interior design, furniture building, and artistic expression.

Product Description

Product Definition

 

Veropoxy is specially formulated for marble slabs, epoxy resin is a premium two-component adhesive designed to provide unrivalled protection and enhancement of natural stone. This epoxy resin offers a firm protective layer that improves marble’s abrasion and chemical resistance while also brilliantly highlighting its original texture and color from great clarity and gloss. It is simple to apply and fixes on a smooth surface that not only accentuates marble’s beauty but also significantly increases its durability. Perfect for interior design, furniture building, and artistic expression, Veropoxy gives marble slabs a contemporary and enduring appeal. Select Veropoxy to provide your marble slab project professional-grade protection and beauty.

marble

 

Product Features

Feature Epoxy Resin for  Gray Marble
Applicable material Diano Real Gray Marble,Venetian Brown
Epoxy system code 4099+B25Q-KG
Epoxy system ratio by weight 100:25
Curing effect Forms a liquid sealing layer
Durability High stability and long-lasting after curing,good yellowing resistance , low viscosity , strong Bonding
Ease of Use Easy to mix and apply, no special tools required

Highlights of the product

 

* Simple User Interface
Perfect texture, handy 1:1 ratio, simple use for beginners and experts. Working doesn’t call for wearing a mask.

 

* Safety First
Made with premium non-toxic components 100% safe for indoor and outdoor usage, transparent epoxy resin is Not one hazardous chemical, reaction, or fumes!

 

* Powerful UV Resistant Light
Top-grade UV-resistant protective coating offered by self-leveling formula Experience powerful light and great gloss, assured to last a lifetime!

 

Operation stages

 

1: Weigh glue A and glue B according to the specified weight ratio; pour into the ready clean container; twist the mixture clockwise around the container wall to mix completely; let it stand for three to five minutes before use.

 

2. Use glue in line with the useful time and quantity to minimize waste. Please heat glue A to 30℃ when the temperature is less than 15℃ before combining with glue B; the glue must be covered after use to prevent moisture absorption and rejection. The glue will thicken at low temperatures.

 

The surface of the cured mixture will collect air moisture and develop a layer of white mist on top when the relative humidity is higher than 85%. For room temperature curing, then, the relative humidity above 85% is not appropriate. One is advised to use heated cure.

 

 

Application of Epoxy Resin on Marble Slabs

 

  1. Adhesive

Epoxy resin’s strong adhesion makes it ideal for securing marble slabs, ensuring stability in both large projects and small repairs. It bonds marble to various materials, like wood, glass, or metal, and withstands external stress, providing long-term safety.

 

  1. Filling

As a filler, epoxy resin smooths out cracks or holes in marble, enhancing durability and appearance. This repair not only boosts visual appeal but also reinforces structural stability, preventing future damage.

 

  1. Surface Coating

An epoxy coating enhances marble’s look and offers waterproof, stain-resistant protection, preserving marble’s shine and simplifying maintenance. Ideal for kitchens, bathrooms, and public spaces, it helps marble retain its natural charm across various settings.

 

  1. Decorative Value

Epoxy resin’s versatility in design allows for unique visual effects. Whether for custom furniture or art, it adds charm, adapting to both minimalist and traditional aesthetics.

 

  1. Chemical and Heat Resistance

With high resistance to chemicals and heat, epoxy resin protects marble in areas like bathrooms and kitchens. It prevents damage from cleaners and oils, maintaining marble’s appearance and reducing future maintenance needs.

 

  1. Protection and Restoration

Epoxy resin extends marble’s life by minimizing wear and scratches, helping it maintain its natural luster. Regular treatment prevents minor damage from worsening, keeping marble looking pristine.

 

  1. Environmentally Friendly Properties

Modern, low-VOC epoxy resins reduce indoor air impact, making them environmentally friendly and suitable for interiors. This option supports sustainable development while preserving marble’s beauty and durability.

 

With this introduction, you can fully understand the product features and usage methods of the Epoxy Resin Sealant for Marble. We are committed to providing high-quality products to meet your needs for the maintenance and repair of Marble.

Get A Free Quote
Contact us for free quotes and more professional knowledge about product. We will prepare a professional solution for you.


    Leave Your Message

      * Name

      * Email

      Phone/WhatsAPP/WeChat

      * What I have to say